Polymer Property : 100% Modulus = 0.00580 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00580 GPa
0.841 ksi
ASTM D412
Precision Polymer Engineering Perlast® G74P Translucent Perfluoroelastomer
A translucent beige compound with semi-crystalline perfluoropolymer nano-filler, specially developed to meet the demands of the semiconductor and bio-analytical industries. Compatible with fluorine ..
100% Modulus 0.00580 GPa
0.841 ksi
DIN 53504
Lubrizol ESTANE® T5090 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00580 GPa
0.841 ksi
Cured 10 minutes at 180°C
DuPont Vamac® DP 3.5 phr Peroxide Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
100% Modulus 0.00580 GPa

@Temperature 23.0 °C
0.841 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Arizona
Lubrizol Estane® 58610 Thermoplastic Polyurethane
Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee..
100% Modulus 0.00580 GPa

@Temperature 23.0 °C
0.841 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Ohio
Lubrizol Estane® 58610 Thermoplastic Polyurethane
Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee..
100% Modulus 0.00580 GPa
0.841 ksi
Post cure 2 hours @ 180°C
3M Dyneon™ FPO 3741 Fluoroelastomer
Information provided by the Dyneon division of 3M.
100% Modulus 0.00580 GPa
0.841 ksi
DIN 53504
Lubrizol ESTANE® 58437 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..