Mechanical Properties Metric English Comments
100% Modulus 0.00570 GPa
0.827 ksi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Santoprene® 253-36 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b..
100% Modulus 0.00570 GPa
0.827 ksi
ASTM D412
DuPont Vamac® G/HVG Sample Compound  (discontinued **)
Test compound is press cured for 5 minutes at 175°C and post cured for 4 hours at 175°C.Information provided by DuPont.
100% Modulus 0.00570 GPa
0.827 ksi
DIN 53504
Huntsman IROGRAN® A 80 P 4699L Ether-Based TPU-For Cable Industry
Introduction: IROGRAN A 80 P 4699 L is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection mold applications. IROGRAN A 80 P 4699 L is part of the HUNT..
100% Modulus 0.00570 GPa
0.827 ksi
DIN 53504
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00570 GPa

@Temperature 23.0 °C
0.827 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Florida
Lubrizol Estane® 58610 Thermoplastic Polyurethane
Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee..
100% Modulus 0.00570 GPa
0.827 ksi
DIN 53504
Lubrizol ESTANE® 58562 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..