Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00569 GPa | 0.825 ksi | ASTM D-638 |
Axiall 83-126J Moldings & Extrusions Flexible PVC Flame retardant, 60°C rated injection molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |