Axiall 83-126J Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 83-126J Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant, 60°C rated injection molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.44 - 1.48 g/cc
1.44 - 1.48 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 73 - 79
73 - 79
delayed; ASTM D-2240
Tensile Strength, Yield 7.24 MPa
1050 psi
ASTM D-638
Elongation at Yield 225 %
225 %
ASTM D-638
100% Modulus 0.00569 GPa
0.825 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -30.0 °C
-22.0 °F
ASTM D-746
Oxygen Index 26 %
26 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 166 °C
330 °F