Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 0.00510 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00510 GPa
0.740 ksi
ASTM D412
SK Chemicals SKYTHANE® S180A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
100% Modulus 0.00510 GPa
0.740 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3480N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
100% Modulus 0.00510 GPa
0.740 ksi
ASTM D412
Lubrizol STAT-RITE® E-1140 Ester-Type Static Dissipative Polymer
Description: Stat-Rite® E-1140 is a static dissipative thermoplastic polyurethane (TPU) alloy. Stat-Rite E-1140 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to ..
100% Modulus 0.00510 GPa
0.740 ksi
DuPont Vamac® G Sample Compound Vulcanizate Slab Cure (10 minutes at 177°C)
Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for their own applications.Information provided by DuPont.
100% Modulus 0.00510 GPa
0.740 ksi
DuPont Vamac® GXF Sample Compound Vulcanizate Slab Cure (5 minutes at 190°C) Without Armeen® 18D
Test slab is cured for 5 minutes at 190°C and post cured for 4hrs at 175°C. Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for their own ..
100% Modulus 0.00510 GPa
0.740 ksi
ISO 37
ELASTO UK Dryflex® 5049-110 TPE, Modified Injection Molding Grade for Auto Mud Flaps
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 5049-110 is specifically designe..
100% Modulus 0.00510 GPa
0.740 ksi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 4680 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
100% Modulus 0.00510 GPa
0.740 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer
A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj..
100% Modulus 0.00510 GPa
0.740 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer
A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex..
100% Modulus 0.00510 GPa
0.740 ksi
DIN 53504
Lubrizol ESTANE® 54620 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..