Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00462 GPa | 0.670 ksi | ASTM D412 |
Huntsman IROGRAN® PS 440-200 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |