Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman IROGRAN® PS 440-200 TPU-Polyester

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Huntsman Corporation
Trade Name IROGRAN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman IROGRAN® PS 440-200 TPU-Polyester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
ASTM D2240
Hardness, Shore D 43
43
ASTM D2240
Tensile Strength at Break 49.4 MPa
7170 psi
ASTM D412
Elongation at Break 490 %
490 %
ASTM D412
50% Modulus 0.00386 GPa
0.560 ksi
ASTM D412
100% Modulus 0.00462 GPa
0.670 ksi
ASTM D412
300% Modulus 0.0152 GPa
2.21 ksi
ASTM D412
Rebound 36 %
36 %
Bayshore; ASTM D2632
Tear Strength 87.7 kN/m
500 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 18
18
ASTM D3389
Abrasion 28
28
mm<sup>3</sup>; DIN 53516
Compression Set 30 %

@Temperature 22.8 °C,
Time 79200 sec
30 %

@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395
80 %

@Temperature 70.0 °C,
Time 79200 sec
80 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Melting Point 159 - 176 °C
318 - 349 °F
TMA Melt Range
Vicat Softening Point 89.0 °C
192 °F
ASTM D1525
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
Midpoint; ASTM E 1269
Users viewing this material also viewed the following: