Mechanical Properties Metric English Comments
100% Modulus 0.00359 GPa
0.520 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00359 GPa
0.520 ksi
ASTM D412
SK Chemicals SKYTHANE® S175A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
100% Modulus 0.00359 GPa
0.520 ksi
ASTM D412
Teknor Apex UNIPRENE® 7010-73 Thermoplastic Elastomer
Information provided by Teknor Apex Company
100% Modulus 0.00359 GPa
0.520 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00359 GPa
0.520 ksi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Advanced Polymer Alloys Alcryn® 2070 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
100% Modulus 0.00359 GPa
0.520 ksi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 2265 UT Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
100% Modulus 0.00359 GPa
0.520 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2122 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FC 2122 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..