Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00214 GPa | 0.310 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-990 (MT) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00214 GPa | 0.310 ksi | ASTM D412 |
Teknor Apex Uniprene® 55A Polyvinyl Chloride, Flexible Features: High Elastic RecoveryInformation Provided by Teknor Apex |
|||
100% Modulus | 0.00214 GPa | 0.310 ksi | ASTM D412 |
Teknor Apex UNIPRENE® 7100-55 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.00214 GPa | 0.310 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-990 (MT) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |