Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00162 GPa | 0.235 ksi | Injection molded plaques, Die C, Cross Direction; ASTM D412 |
Kraton® G2705 GU (SEBS) Compound Description: Kraton G2705 GU-N is an easy processing material designed for applications where FDA regulations are required. The material exhibits high resilience, low compression set, and good punct.. |
|||
100% Modulus | 0.00162 GPa | 0.235 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 30.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
100% Modulus | 0.00162 GPa | 0.235 ksi | ASTM D638 |
Colorite Polymers 3511-02 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00162 GPa | 0.235 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 30.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |