Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00145 GPa | 0.211 ksi | ASTM D412 |
Northstar Polymers MPP-A50A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
100% Modulus | 0.00145 GPa | 0.210 ksi | heat aged one week at 300ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00145 GPa | 0.210 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 15.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
100% Modulus | 0.00145 GPa | 0.210 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N990 (MT) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00145 GPa | 0.210 ksi | ASTM D412 |
Huntsman IROGRAN® PS 370-202 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
100% Modulus | 0.00145 GPa | 0.210 ksi | heat aged one week at 300ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00145 GPa | 0.210 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 15.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
100% Modulus | 0.00145 GPa | 0.210 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N990 (MT) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |