Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hydrostatic Design Basis | 9.65 MPa | 1400 psi | Hydrostatic Crush Strength (3200 feet) |
Engineered Syntactic Systems PSF-42 Polyester Subsea Syntactic Void Filler PSF-42 was developed by Navy subcontractors for simple shipyard-based cavity pours of Naval vessels. This system may be used in any free-flood cavity or void, but is especially valuable in difficult.. |