Material Notes:
PSF-42 was developed by Navy subcontractors for simple shipyard-based cavity pours of Naval vessels. This system may be used in any free-flood cavity or void, but is especially valuable in difficult-to-fill cavities and in circumstances where quick working time is required. The mix is a low viscosity, multicomponent, fast cure system that cures at room temperature to form a solid syntactic material that will easily perform at depths of 1,500 feet.
Physical Properties Metric English Comments
Density <= 0.705 g/cc
<= 0.0255 lb/in³
Water Absorption <= 3.0 %

@Time 86400 sec
<= 3.0 %

@Time 24.0 hour
Mechanical Properties Metric English Comments
Compressive Strength >= 27.6 MPa
>= 4000 psi
Compressive Modulus >= 1.72 GPa
>= 250 ksi
Hydrostatic Design Basis 9.65 MPa
1400 psi
Hydrostatic Crush Strength (3200 feet)
Descriptive Properties Value Comments
Color White/Tan