Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 10.8 J

@Temperature 23.0 °C
8.00 ft-lb

@Temperature 73.4 °F
Instrument Impact, Total Energy; ASTM D3763
ExxonMobil Escorene® LD 783.ND Molding, extrusion and compounding resin  (discontinued **)
Escorene Ultra LD 783.ND is a 33% vinyl acetate copolymer suitable for making a variety of specialty molding and extrusion compounds. It has high clarity and a very low modulus.Information provided ..