Mechanical Properties Metric English Comments
Impact Test 78.0 J

@Temperature 23.0 °C
57.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region.
Impact Test 78.0 J

@Temperature 23.0 °C
57.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 78.0 J

@Temperature 23.0 °C
57.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 78.0 J

@Temperature 23.0 °C
57.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region.
Impact Test 78.0 J

@Temperature 23.0 °C
57.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 78.0 J

@Temperature 23.0 °C
57.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg..