Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 67.8 J @Thickness 3.17 mm, Temperature -40.0 °C |
50.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
rotomolded; ARM Method |
NOVA Chemicals Novapol® TR-0735-U Hexene MDPE Rotational Molding Resin Good impact resistance, Excellent processabilityApplications: Toys, Complex custom parts, Home and garden items, MailboxesAdditives: Processing antioxidants, UV stabilizersInformation provided by NO.. |
|||
Impact Test | 67.8 J @Thickness 3.17 mm |
50.0 ft-lb @Thickness 0.125 in |
ARM Method |
NOVA Chemicals Novapol® TR-0735-UG Hexene MDPE Rotational Molding Resin Features: Good impact properties Excellent processabilityNSF listed for Stds. 14, 24 and 61 Applications: ToysComplex custom partsHome and garden itemsMailboxesInformation provided by Nova Chemicals.. |
|||
Impact Test | 67.8 J @Thickness 3.17 mm, Temperature -40.0 °C |
50.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
rotomolded; ARM Method |
NOVA Chemicals Sclair® 8107 UV8D Butene LLDPE Rotational Molding Resin Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listedApplications: Food and laundry materials handlin.. |
|||
Impact Test | 67.8 J @Temperature -30.0 °C |
50.0 ft-lb @Temperature -22.0 °F |
Instrumented Dart Total Energy |
Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified
(discontinued **) ISOPLAST® 151 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois.. |
|||
Impact Test | 67.8 J @Temperature 23.0 °C |
50.0 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified
(discontinued **) ISOPLAST® 151 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois.. |
|||
Impact Test | 67.8 J @Thickness 3.17 mm, Temperature -40.0 °C |
50.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
Rotomolded samples; ARM Method |
NOVA Chemicals Novapol® TR-0535-UI Hexene MDPE Rotational Molding Resin TR-0530-UI complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. TR-0530-UI is su.. |
|||
Impact Test | 67.8 J @Thickness 3.17 mm, Temperature -40.0 °C |
50.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
Rotomolded samples; ARM Method |
NOVA Chemicals Novapol® TR-0535-UIG Hexene MDPE Rotational Molding Resin TR-0530-UIG complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. TR-0530-UIG is .. |
|||
Impact Test | 67.8 J @Thickness 3.17 mm, Temperature -40.0 °C |
50.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
rotomolded; ARM Method |
NOVA Chemicals Sclair® 8107G UV8D Butene LLDPE Rotational Molding Resin Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listedApplications: Food and laundry materials handlin.. |
|||
Impact Test | 67.8 J @Thickness 3.17 mm, Temperature -40.0 °C |
50.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
rotomolded; ARM Method |
NOVA Chemicals Novapol® PR-0636-UG Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |
|||
Impact Test | 67.8 J @Thickness 3.17 mm, Temperature -40.0 °C |
50.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
rotomolded; ARM Method |
NOVA Chemicals Sclair® TD-7915-UG Hexene MDPE Rotational Molding Resin
(discontinued **) Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera.. |
|||
Impact Test | 67.8 J @Temperature -30.0 °C |
50.0 ft-lb @Temperature -22.0 °F |
Instrumented Dart Total Energy |
Dow Prevail® 3050 ABS + Polyurethane PREVAIL® 3050 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |
|||
Impact Test | 67.8 J @Thickness 3.17 mm, Temperature -40.0 °C |
50.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
rotomolded; ARM Method |
NOVA Chemicals Sclair® TD-7915-U Hexene MDPE Rotational Molding Resin
(discontinued **) Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera.. |
|||
Impact Test | 67.8 J @Thickness 3.17 mm, Temperature -40.0 °C |
50.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
rotomolded; ARM Method |
NOVA Chemicals Novapol® PR-0636-U Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |