Mechanical Properties Metric English Comments
Impact Test 47.0 J

@Temperature 23.0 °C
34.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS
Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Americas region.
Impact Test 47.0 J

@Temperature 23.0 °C
34.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS (Asia Pacific)
Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 47.0 J

@Temperature 23.0 °C
34.7 ft-lb

@Temperature 73.4 °F
3.2 mm, 2.2m/s. Instrumented Impact; ASTM D 3763
MRC Polymers NAXELLâ„¢ PC429MHI Polycarbonate, Impact Modified
• Medium MFR• Good property retention, heat and dimensional stability• Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants ca..
Impact Test 47.0 J

@Temperature -40.0 °C
34.7 ft-lb

@Temperature -40.0 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xenoy® 364 PBT
This data was supplied by SABIC-IP for the Americas region.
Impact Test 47.0 J

@Temperature 23.0 °C
34.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xenoy® 364 PBT
This data was supplied by SABIC-IP for the Americas region.
Impact Test 47.0 J

@Temperature -40.0 °C
34.7 ft-lb

@Temperature -40.0 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Valox® 364 PBT
Designed for outdoor telecommunications enclosure applications.This data was supplied by SABIC-IP for the Americas region.