Mechanical Properties Metric English Comments
Impact Test 4.00 J

@Temperature -30.0 °C
2.95 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
Dow Retain® 8209 ABS + Polycarbonate
Data provided by Dow Chemical.
Impact Test 4.00 J

@Temperature 23.0 °C
2.95 ft-lb

@Temperature 73.4 °F
Multi-axial, at failure, measured on flat plaques; ASTM D3763
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Impact Test 4.00 J

@Temperature 23.0 °C
2.95 ft-lb

@Temperature 73.4 °F
Multi-axial, at max. load; ASTM D3763
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)
AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Impact Test 4.00 J

@Temperature 23.0 °C
2.95 ft-lb

@Temperature 73.4 °F
Multi-axial, at max. load; ASTM D3763
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)
AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..