Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Impact Test = 33.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 33.0 J

@Temperature 23.0 °C
24.3 ft-lb

@Temperature 73.4 °F
Multiaxial Impact (3.4 m/s, 40-mm ring, M831 Striker); Total Energy; ASTM-D3763
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade
Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components.
Impact Test 33.0 J

@Temperature 23.0 °C
24.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
Diamond Polymers Centrex® 813 General Purpose Injection Molding Grade ASA/AES
Centrex 813 resin is a high-gloss, high-impact grade of ASA/AES, a blend of acrylonitrile-styrene-acrylate and acrylonitrile-ethylene-propylene styrene. This injection molding grade with a good bala..
Impact Test 33.0 J

@Temperature 23.0 °C
24.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
Diamond Polymers Centrex® 814 General Purpose Injection Molding Grade
Centrex 814 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and processing perfor..
Impact Test 33.0 J

@Temperature 23.0 °C
24.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
Diamond Polymers Centrex® 821 ASA Weatherable Polymers Injection Molding Grade
Centrex 821 resin is a medium-gloss, high-heat, medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and pr..
Impact Test 33.0 J

@Thickness 6.00 mm
24.3 ft-lb

@Thickness 0.236 in
ASTM D2794-93
3M Scotchkote™ 2400 Pipe Renewal Liner
3M Scotchkote Pipe Renewal Liner 2400 has been specifically developed for the rehabilitation of potable water pipe infrastructure to help extend service life, reduce leaks, and improve water quality..