Material Notes:
3M Scotchkote Pipe Renewal Liner 2400 has been specifically developed for the rehabilitation of potable water pipe infrastructure to help extend service life, reduce leaks, and improve water quality by preventing the future build-up of tuberculation that can lead to color, taste, and odor issues. Scotchkote Liner 2400 should be specified at an appropriate caliper thickness contingent upon pipe condition, pipe diameter, bury depth, target design life, safety design factor and host pipe material substrate type. Consult the Scotchkote Liner 2400 Design and Installation Guide for engineering design considerations. At prescribed caliper thickness, Scotchkote Liner 2400 is project to meet material properties of ASTM F1216-09 after 50 years. 3M used the following test methods to validate: ASTM D638-08, ASTM D790-07, ASTM D2990-08 and ASTM D1599-99.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Water Absorption 1.31 %
1.31 %
21 days; ASTM D570-98
Mechanical Properties Metric English Comments
Hardness, Shore D 87
87
ASTM D2240-5
Tensile Strength at Break 39.0 MPa
5660 psi
ASTM D638-08
Elongation at Break 5.0 %
5.0 %
ASTM D638-08
Flexural Strength 58.0 MPa
8410 psi
ASTM D790-07
Flexural Modulus 3.62 GPa
525 ksi
ASTM D790-07
Impact Test 17.0 J

@Thickness 1.70 mm
12.5 ft-lb

@Thickness 0.0669 in
ASTM D2794-93
33.0 J

@Thickness 6.00 mm
24.3 ft-lb

@Thickness 0.236 in
ASTM D2794-93
Abrasion 193
193
[mg] loss per 1000 cycles; ASTM D4060-07
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 96.0 °C
205 °F
ASTM D70207
Electrical Properties Metric English Comments
Dielectric Strength 15.7 kV/mm
400 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 10.0 min
0.167 hour
for CCTV Inspection
60.0 min
1.00 hour
Total Cure
Gel Time 1.00 min
1.00 min
Shelf Life 12.0 Month

@Temperature 5.00 - 32.0 °C
12.0 Month

@Temperature 41.0 - 89.6 °F
Descriptive Properties Value Comments
Appearance Gray