Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Impact Test = 28.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 38.0 J

@Temperature -40.0 °C
28.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
ExxonMobil Escorene® LD 767.MJ Molding, extrusion and compounding resin  (discontinued **)
Escorene Ultra LD 767.MJ is a high viscosity, 29.5% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be ..
Impact Test 38.0 J

@Temperature 23.0 °C
28.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
Diamond Polymers Centrex® 601 Profile Extrusion Grade AES
Centrex 601 resin is a very high-impact, low-gloss AES (acrylonitrile-ethylene-propylene-styrene) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can..
Impact Test 38.0 J

@Temperature 23.0 °C
28.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
Diamond Polymers Centrex® 825 Sheet Extrusion Grade
Centrex 825 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it ..
Impact Test 38.0 J

@Temperature -18.0 °C
28.0 ft-lb

@Temperature -0.400 °F
ASTM D3763
Diamond Polymers Centrex® 833 Sheet Extrusion Grade
Centrex 833 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it ..
Impact Test 38.0 J

@Thickness 4.00 mm
28.0 ft-lb

@Thickness 0.157 in
Multi-axial, at max. load; ASTM D3763
Azdel Plus U421-B01 42% Directionalized Continuous Fiber Mat / PP Resin Matrix
AZDEL® U421-B01 is a glass mat thermoplastic laminate based upon a combination of random oriented continuous fiber mat and oriented fiber mat contained within a polypropylene resin matrix. This co..
Copyright © lookpolymers.com All Rights Reserved