Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 38.0 J @Temperature -40.0 °C |
28.0 ft-lb @Temperature -40.0 °F |
Instrumented Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 767.MJ Molding, extrusion and compounding resin
(discontinued **) Escorene Ultra LD 767.MJ is a high viscosity, 29.5% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be .. |
|||
Impact Test | 38.0 J @Temperature 23.0 °C |
28.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Diamond Polymers Centrex® 601 Profile Extrusion Grade AES Centrex 601 resin is a very high-impact, low-gloss AES (acrylonitrile-ethylene-propylene-styrene) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can.. |
|||
Impact Test | 38.0 J @Temperature 23.0 °C |
28.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Diamond Polymers Centrex® 825 Sheet Extrusion Grade Centrex 825 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it .. |
|||
Impact Test | 38.0 J @Temperature -18.0 °C |
28.0 ft-lb @Temperature -0.400 °F |
ASTM D3763 |
Diamond Polymers Centrex® 833 Sheet Extrusion Grade Centrex 833 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it .. |
|||
Impact Test | 38.0 J @Thickness 4.00 mm |
28.0 ft-lb @Thickness 0.157 in |
Multi-axial, at max. load; ASTM D3763 |
Azdel Plus U421-B01 42% Directionalized Continuous Fiber Mat / PP Resin Matrix AZDEL® U421-B01 is a glass mat thermoplastic laminate based upon a combination of random oriented continuous fiber mat and oriented fiber mat contained within a polypropylene resin matrix. This co.. |