Polymer Property : Impact Test = 244 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 244 J

@Thickness 6.35 mm,
Temperature -40.0 °C
180 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
rotomolded; ARM Method
NOVA Chemicals Novapol® TR-0242-U MDPE Rotational Molding Resin  (discontinued **)
Hexene copolymer, Excellent impact, Excellent ESCRApplications: Large parts, Agricultural storage tanksAdditives: Processing antioxidants, UV stabilizersInformation provided by NOVA Chemicals.
Impact Test 244 J

@Thickness 6.35 mm,
Temperature -40.0 °C
180 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM Impact
Chevron Phillips Marlex® HMN TR-942/942G Polyethylene; HDPE
High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and fair flowLong-term UV stabilizationExcellent impact stren..
Impact Test 244 J

@Thickness 6.35 mm,
Temperature 25.0 °C
180 ft-lb

@Thickness 0.250 in,
Temperature 77.0 °F
ARM
ExxonMobil HD 8660.29 Rotational Molding Resin
Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o..
Impact Test 244 J

@Thickness 6.35 mm,
Temperature 25.0 °C
180 ft-lb

@Thickness 0.250 in,
Temperature 77.0 °F
ARM
ExxonMobil HDP8660.29 Rotational Molding Resin
Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o..
Impact Test 244 J

@Thickness 6.35 mm,
Temperature -40.0 °C
180 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
rotomolded; ARM Method
NOVA Chemicals Novapol® TR-0242-UG MDPE Rotational Molding Resin  (discontinued **)
Hexene copolymer, Excellent impact, Excellent ESCRApplications: Large parts, Agricultural storage tanksAdditives: Processing antioxidants, UV stabilizersInformation provided by NOVA Chemicals.