Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 244 J @Thickness 6.35 mm, Temperature -40.0 °C |
180 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
rotomolded; ARM Method |
NOVA Chemicals Novapol® TR-0242-U MDPE Rotational Molding Resin
(discontinued **) Hexene copolymer, Excellent impact, Excellent ESCRApplications: Large parts, Agricultural storage tanksAdditives: Processing antioxidants, UV stabilizersInformation provided by NOVA Chemicals. |
|||
Impact Test | 244 J @Thickness 6.35 mm, Temperature -40.0 °C |
180 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
ARM Impact |
Chevron Phillips Marlex® HMN TR-942/942G Polyethylene; HDPE High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and fair flowLong-term UV stabilizationExcellent impact stren.. |
|||
Impact Test | 244 J @Thickness 6.35 mm, Temperature 25.0 °C |
180 ft-lb @Thickness 0.250 in, Temperature 77.0 °F |
ARM |
ExxonMobil HD 8660.29 Rotational Molding Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Impact Test | 244 J @Thickness 6.35 mm, Temperature 25.0 °C |
180 ft-lb @Thickness 0.250 in, Temperature 77.0 °F |
ARM |
ExxonMobil HDP8660.29 Rotational Molding Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Impact Test | 244 J @Thickness 6.35 mm, Temperature -40.0 °C |
180 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
rotomolded; ARM Method |
NOVA Chemicals Novapol® TR-0242-UG MDPE Rotational Molding Resin
(discontinued **) Hexene copolymer, Excellent impact, Excellent ESCRApplications: Large parts, Agricultural storage tanksAdditives: Processing antioxidants, UV stabilizersInformation provided by NOVA Chemicals. |