Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 31.2 J @Temperature -40.0 °C |
23.0 ft-lb @Temperature -40.0 °F |
Instrumented Impact, Total Energy; ASTM D3763 |
ExxonMobil OPTEMA™ TC 115 Molding, extrusion and compounding resin
(discontinued **) OPTEMA TC 115 is an ethylene methyl acrylate copolymer, which can be used as a compatibilizer and impact modifier for engineering thermoplastics. It has been processed at temperatures up to 625°F w.. |
|||
Impact Test | 31.2 J @Temperature -40.0 °C |
23.0 ft-lb @Temperature -40.0 °F |
Instrumented Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 768.MJ Molding, extrusion and compounding resin Escorene Ultra LD 768.MJ is a high viscosity, 26.2% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be .. |