Polymer Property : Impact Test = 16.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 16.0 J

@Temperature -18.0 °C
11.8 ft-lb

@Temperature -0.400 °F
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Total Energy; ASTM-D3763
Ineos ABS Lustran® 256 Extrusion Blending Grade
Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi..
Impact Test 16.0 J

@Temperature 23.0 °C
11.8 ft-lb

@Temperature 73.4 °F
Multi-Axial Impact, Fractovis J; Energy Peak; ASTM-D3763
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade
Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®..
Impact Test 16.0 J

@Temperature -30.0 °C
11.8 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 347EZ ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 16.0 J

@Temperature 23.0 °C
11.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Verton RV008ESV_GY7E072 PA 66
Preliminary data for 40% long glass fiber filled, single color pellet gray, PA66This data was supplied by SABIC-IP for the Americas region.
Impact Test 16.0 J

@Temperature -18.0 °C
11.8 ft-lb

@Temperature -0.400 °F
ASTM D3763
Diamond Polymers Centrex® 485 Sheet Extrusion Grade
Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it..
Impact Test 16.0 J

@Treatment Temp. 400 °C
11.8 ft-lb

@Treatment Temp. 752 °F
400°C Tempering temperature (2h + 2h)
Assab Steels 8407 SUPREME Hot Work Steel
8407 SUPREME is characterized by:High level of resistance to thermal shock and thermal fatigueGood high temperature strengthExcellent toughness and ductility in all directionsGood machinability and ..