Izod Impact Unnotched 51.5 J
38.0 ft-lb
Oil Quenched at 1218°C; 580°C Temper Temperature
Latrobe Tatmoâ„¢ ASTM M1 High Speed Steel
TATMO is an M1-type, general-purpose high speed steel. In comparison with other popular high speed steels, it exhibits excellent toughness and grindability. These factors and its relatively low cost..
Izod Impact Unnotched 51.5 J
38.0 ft-lb
Oil Quenched at 1232°C; 482°C Temper Temperature
Latrobe Double Six™ ASTM M2 High Speed Steel
DOUBLE SIX (M2) is a tungsten-molybdenum high speed steel with a well balanced composition suitable for a wide variety of applications. World wide, the M2 type is by far the most popular high speed ..