Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 51.5 J | 38.0 ft-lb | Oil Quenched at 1218°C; 580°C Temper Temperature |
Latrobe Tatmoâ„¢ ASTM M1 High Speed Steel TATMO is an M1-type, general-purpose high speed steel. In comparison with other popular high speed steels, it exhibits excellent toughness and grindability. These factors and
its relatively low cost.. |
|||
Izod Impact Unnotched | 51.5 J | 38.0 ft-lb | Oil Quenched at 1232°C; 482°C Temper Temperature |
Latrobe Double Six™ ASTM M2 High Speed Steel DOUBLE SIX (M2) is a tungsten-molybdenum high speed steel with a well balanced composition suitable for a wide variety of applications. World wide, the M2 type is by far
the most popular high speed .. |