Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact Unnotched = 47.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Unnotched 63.7 J
47.0 ft-lb
Oil Quenched at 1175°C; 622°C Temper Temperature
Latrobe CM-52â„¢ ASTM M52 High Speed Steel
CM-52 is classified as an intermediate type high speed steel of the molybdenum chromium-vanadium variety. It is recommended for intermediate cutting applications such as commercial twist drills and ..
Izod Impact Unnotched 63.7 J
47.0 ft-lb
Oil Quenched at 1177°C; 566°C Temper Temperature
Latrobe Corsairâ„¢ ASTM M3-1 High Speed Steel
CORSAIR (M3-1) contains carbon and vanadium levels that are intermediate between those of Double Six (M2) and Crusader (M3-2). This gives the steel a fine balance of wear resistance and grindability..