Mechanical Properties Metric English Comments
Izod Impact Unnotched 27.1 J
20.0 ft-lb
Oil Quenched from 788°C; 250°C Temper Temperature
Latrobe Graph-Mo® Cold Work Tool Steel (ASTM O6)
Graph-Mo tool steel is an oil-hardening, graphitic tool steel with outstanding resistance to metal-to-metal sliding wear and galling. The steel contains a uniform dispersion of graphite particles wh..
Izod Impact Unnotched 27.1 - 46.1 J
20.0 - 34.0 ft-lb
Carpenter Micro-Melt® T-15 Alloy (AISI T15)
Micro-Melt® T-15 alloy is a high-carbon tungsten-cobalt-vanadium high speed powder metal tool steel possessing excellent abrasion resistance and red hardness. The advantages of Micro-Melt premium p..
Izod Impact Unnotched 27.1 J
20.0 ft-lb
Oil Quenched from 816°C; 150°C Temper Temperature
Latrobe LSS™ O1 Tool Steel (ASTM O1)
TLS O1 tool steel is the original oil-hardening, "non-shrinking" tool steel that can be hardened to the Rockwell C 65 range from a low austenitizing temperature. TLS O1 is a general-purpose tool ste..