Carpenter Micro-Melt® T-15 Alloy (AISI T15)

Category Metal , Ferrous Metal , Carbon Steel , High Carbon Steel , Tool Steel
Manufacturer Carpenter Technology Corporation (Cartech)
Trade Name Micro-Melt®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carpenter Micro-Melt® T-15 Alloy (AISI T15).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Micro-Melt® T-15 alloy is a high-carbon tungsten-cobalt-vanadium high speed powder metal tool steel possessing excellent abrasion resistance and red hardness. The advantages of Micro-Melt premium powder high speed steels include ease of grinding, response to heat treatment, more uniform structure, greater wear resistance and improved toughness. In addition, Carpenter's unique hot rolling and rotary forging capabilities impart minimal distortion characteristics to these alloys.Applications: Form tools, Lathe tools, Planer tools, Broaches, Milling cutters, Blanking dies, Punches, Drills, Screw machine tools, Cold work toolsInformation provided by Carpenter Technology Corporation.Micro-Melt® is a registered trademark of Carpenter Technology Corporation.
Physical Properties Metric English Comments
Specific Gravity 8.19 g/cc
8.19 g/cc
Mechanical Properties Metric English Comments
Hardness, Rockwell C 46.5
46.5
Tempered at 1275°F
67.5
67.5
Tempered at 1025°F
Modulus of Elasticity 200 - 207 GPa
29000 - 30000 ksi
Izod Impact Unnotched 27.1 - 46.1 J
20.0 - 34.0 ft-lb
Abrasion 8.0
8.0
loss in mm<sup>3</sup>, Tempered at 1025°F; ASTM G65
32.3
32.3
loss in mm<sup>3</sup>, Tempered at 1275°F; ASTM G65
Thermal Properties Metric English Comments
CTE, linear 9.93 µm/m-°C

@Temperature 37.8 - 260 °C
5.52 µin/in-°F

@Temperature 100 - 500 °F
11.95 µm/m-°C

@Temperature 37.8 - 816 °C
6.639 µin/in-°F

@Temperature 100 - 1500 °F
Component Elements Properties Metric English Comments
Carbon, C 1.5 %
1.5 %
Chromium, Cr 4.75 %
4.75 %
Cobalt, Co 5.0 %
5.0 %
Iron, Fe 70.69 %
70.69 %
As Balance
Sulfur, S 0.060 %
0.060 %
Tungsten, W 13 %
13 %
Vanadium, V 5.0 %
5.0 %