Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 65.5 MPa | 9500 psi | Ultimate; TM R050-38 |
Resinlab® EP1285HD-16 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Compressive Strength | 65.5 MPa | 9500 psi | ASTM D-695 |
CMT Materials REN Shape® 470 Tooling Board, Modeling Board, Adhesive Products CMT Materials offers the complete line of REN Shape tooling board, modeling board, and related adhesive products. Vacuum formers and thermoformers use these products as prototype and low volume prod.. |
|||
Compressive Strength | 65.5 MPa | 9500 psi | Break; TM R050-38 |
Resinlab® SEC1222 Silver Filled Epoxy Adhesive Resinlab™ SEC1222 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1222 provides excellent electrical conductivit.. |