Polymer Property : Compressive Strength = 9.65 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 9.65 MPa
1400 psi
ASTM D-695
CMT Materials REN Shape® 440 Tooling Board, Modeling Board, Adhesive Products
CMT Materials offers the complete line of REN Shape tooling board, modeling board, and related adhesive products. Vacuum formers and thermoformers use these products as prototype and low volume prod..