Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CMT Materials REN Shape® 440 Tooling Board, Modeling Board, Adhesive Products

Category Polymer
Manufacturer CMT Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMT Materials REN Shape® 440 Tooling Board, Modeling Board, Adhesive Products.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CMT Materials offers the complete line of REN Shape tooling board, modeling board, and related adhesive products. Vacuum formers and thermoformers use these products as prototype and low volume production molds when forming in applications where metal molds do not makes sense due to time or cost considerations. CMT can help in selecting the proper board material for specific forming applications considering factors such as surface quality, ease in machining, tool durability, and forming temperature.Information Provided by CMT Materials, Inc.
Physical Properties Metric English Comments
Density 0.545 g/cc
0.0197 lb/in³
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 54
54
ASTM D-2240
Tensile Strength, Ultimate 8.96 MPa
1300 psi
ASTM D-638
Flexural Strength 15.9 MPa
2300 psi
ASTM D-790
Flexural Modulus 0.731 GPa
106 ksi
ASTM D-790
Compressive Strength 9.65 MPa
1400 psi
ASTM D-695
Compressive Modulus 0.724 GPa
105 ksi
ASTM D-695
Thermal Properties Metric English Comments
CTE, linear 61.9 µm/m-°C
34.4 µin/in-°F
ASTM D-3386
Glass Transition Temp, Tg 95.0 °C
203 °F
ASTM D-4065
Descriptive Properties Value Comments
Color Brown
Copyright © lookpolymers.com All Rights Reserved