Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 6.50 - 9.50 MPa | 943 - 1380 psi | Cold Crushing Strength |
Gouda Vuurvast GI 34 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |