Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 600 MPa | 87000 psi | |
GBC Cerasilâ„¢ 223U Ceramic Has a lower CTE, better thermal shock resistance, lower firing temperature, and lower consistent shrinkage than steatite.Applications: ideal for volume production of small pressed insulators often r.. |
|||
Compressive Strength | 600 MPa | 87000 psi | |
GBC L3 Steatite Ideal for high frequency, low loss, high voltage insulation. Much less expensive than alumina insulatorsApplications: resistor forms, surge arrestors, standoffs, spacers, and coil forms.Machinabili.. |
|||
Compressive Strength | 600 MPa @Thickness >=5.00 mm |
87000 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax EP S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good electrical and mechanical properties by continuous use, even at high temperatures. Very good chemical resistance. Engineering and insulation material in electrical mac.. |