Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 86.9 MPa | 12600 psi | |
BCC Products BC 7009-2 Epoxy Casting BC 7009-2 is an iron filled, low-cost mass casting system. Recommended for use in casting a minimum of two inches and a maximum of six inches in non-conductive molds. Thicknesses to nine inches in m.. |