Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 590 MPa | 85600 psi | |
ICE Steatite L-5 Data provided by the manufacturer, International Ceramic Engineering. |
|||
Compressive Strength | 590 MPa | 85600 psi | ASTM C773 |
CoorsTek Porcelain Information provided by CoorsTek. |