Compressive Strength 590 MPa
85600 psi
ICE Steatite L-5
Data provided by the manufacturer, International Ceramic Engineering.
Compressive Strength 590 MPa
85600 psi
ASTM C773
CoorsTek Porcelain
Information provided by CoorsTek.