Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 586 MPa @Thickness 12.7 mm |
85000 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP511ES Glass Epoxy Laminate Description: NP511ES is a woven glass fabric with high temperature, static dissipative epoxy resin. It has excellent mechanical strength and electrical properties at elevated temperatures with a con.. |
|||
Compressive Strength | 586 MPa | 85000 psi | |
Du-Co Ceramics DC-200-L-5 Fosterite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |