Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 483 MPa @Thickness 12.7 mm |
70000 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP509 Glass Fabric Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc.. |
|||
Compressive Strength | 483 MPa @Thickness 12.7 mm |
70000 psi @Thickness 0.500 in |
Flatwise |
Industrial Laminates/Norplex P95 Glass Fabric Description: Woven glass fabric with polyimide resin engineered to maintain excellent physical properties at 240°C. Low coefficient of thermal expansion, high mechanical strength.Thickness Tested.. |