Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 7.79 - 7.86 MPa | 1130 - 1140 psi | |
BCC Products MB 1200 Polyurethane Foam Modeling Board MB 1200 is an Apricot and/or Pink colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1200 is low density foam of approximately 20lbs/ft3 board. Easily cut using CNC machining.. |