Polymer Property : Compressive Strength = 1140 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 7.79 - 7.86 MPa
1130 - 1140 psi
BCC Products MB 1200 Polyurethane Foam Modeling Board
MB 1200 is an Apricot and/or Pink colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1200 is low density foam of approximately 20lbs/ft3 board. Easily cut using CNC machining..