Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 68.0 MPa | 9860 psi | 10% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2 Filled, Heat Stabilized, Dry Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 68.0 MPa | 9860 psi | 10% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 68.0 MPa | 9860 psi | 10% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Conditioned Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 68.0 MPa | 9860 psi | 10% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Dry Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 68.0 MPa | 9860 psi | SABIC Method |
SABIC Innovative Plastics LNP LUBRILOY RA2 PA 66 LNP* LUBRILOY* RA2 is a compound based on Nylon 66 resin containing Aramid Fiber. Added feature of this material is: Wear Resistant. |