Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 68.0 MPa
9860 psi
10% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2 Filled, Heat Stabilized, Dry
Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 68.0 MPa
9860 psi
10% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned
Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 68.0 MPa
9860 psi
10% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Conditioned
Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 68.0 MPa
9860 psi
10% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Dry
Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 68.0 MPa
9860 psi
SABIC Method
SABIC Innovative Plastics LNP LUBRILOY RA2 PA 66
LNP* LUBRILOY* RA2 is a compound based on Nylon 66 resin containing Aramid Fiber. Added feature of this material is: Wear Resistant.