Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 67.6 MPa | 9800 psi | ASTM D695 |
Greene Tweed AR™ HT Abrasive-Resistant Thermoplastic ARHT™ is a proprietary thermoplastic material specifically developed for use a sbushings, bearings and wear rings in pumps handling abrasive media up to 250°F (121°C). ARHT provides outs.. |
|||
Compressive Strength | 67.6 MPa | 9800 psi | ASTM D695 |
ITW Devcon Metal Repair Wear Resistant Epoxy (WR-2), Dark Grey Information provided by ITW Devcon |
|||
Compressive Strength | 67.6 MPa | 9800 psi | |
BCC Products BC 5200 Kwik-Set Adhesive BC5200 is a medium viscosity fast gelling two part Epoxy Adhesive System. With an easy to use 1 to 1 mix ratio, BC5200 is considered an excellent general purpose adhesive for in-shop use. BC5200 wil.. |
|||
Compressive Strength | 67.6 MPa | 9800 psi | |
BCC Products BC 8870 Polyurethane Elastomer BC8870 is a low viscosity two-component urethane casting compound that is specifically formulated for high abrasion and impact resistance. It is recommended for use for the production casting of hig.. |