Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 67.2 MPa | 9750 psi | |
BCC Products METAL-KAST/SLO BC 8010-2 Urethane Casting BC8010-2 Metal-Kast/Slo, the result of extensive research and development is an aluminum filled, metal-like, medium setting urethane reproduction plastic. A slower version of the BC8010 Metal-Kast w.. |
|||
Compressive Strength | 67.2 MPa | 9750 psi | ASTM D695 |
BCC Products METAL-KAST BC 8010 Urethane Casting New BC8010 is a quick setting urethane reproduction plastic system that simulates many of the desirable characteristics of aluminum metal. A highly machineable tooling material that is now easier to.. |