Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BCC Products METAL-KAST/SLO BC 8010-2 Urethane Casting

Category Polymer , Thermoset , Polyurethane, TS
Manufacturer BCC Products
Trade Name METAL-KAST/SLO
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products METAL-KAST/SLO BC 8010-2 Urethane Casting.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC8010-2 Metal-Kast/Slo, the result of extensive research and development is an aluminum filled, metal-like, medium setting urethane reproduction plastic. A slower version of the BC8010 Metal-Kast which allows the user longer working time for pouring larger castings or for filling closed mold cavities. BC8010-2 is ideal for the construction of low temperature vacuum form tools, prototypes, models, display parts, patterns, keller aids and bulk back fill.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
Brookfield Viscosity 3250 cP

@Temperature 23.9 °C
3250 cP

@Temperature 75.0 °F
#2 spindle @ 20 rpm
Linear Mold Shrinkage 0.00080 cm/cm
0.00080 in/in
Mechanical Properties Metric English Comments
Hardness, Shore D 85

@Temperature 23.9 °C
85

@Temperature 75.0 °F
Compressive Strength 67.2 MPa
9750 psi
Processing Properties Metric English Comments
Cure Time 360 min

@Temperature 24.0 °C
6.00 hour

@Temperature 75.2 °F
demold time
Pot Life 12 min

@Temperature 24.0 °C
12 min

@Temperature 75.2 °F
1 lb. mass
Descriptive Properties Value Comments
Mix Ratio 1:1 by weight or volume