Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 621 MPa | 90000 psi | 0°, 90° Directions, RT, Dry; ASTM D6641 |
Renegade Materials Corporation RM-5003 Cyanate Ester Prepreg 4581 Quartz Fabric Low dielectric and loss, high performance prepreg. 350°F Cure Developed with consistent handling and superior performance Designed for demanding electrical, radome and antennae applications Del.. |
|||
Compressive Strength | 621 MPa | 90000 psi | |
Meehanite GF-20 Flake Graphite Cast Iron Type GF-20 is designed principally for high machinability and is used where ultimate strength is not an important factor.General Meehanite information - Meehanite metal is first melted to a definite.. |
|||
Compressive Strength | 621 MPa | 90100 psi | |
Du-Co Ceramics CS-144-L-5 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Compressive Strength | 621 MPa | 90000 psi | |
Dura-Bar G1 Continuously Cast Gray Iron Bar Stock ASTM A48 Dura-Bar G1 contains flake graphite in a matrix that is pearlitic with small amounts of ferrite. This is the softest grade of the Dura-Bar gray irons and is normally selected when excellent machinab.. |