Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 6.90 - 12.1 MPa | 1000 - 1750 psi | |
Pyrotek SF-50 Foamed Fused Silica Insulation Board SF-50 is characterized by its uniform open cell structure which allows it to be machined to close tolerances. It can be drilled, sawed or modified with conventional tools. For quick construction o.. |
|||
Compressive Strength | 6.90 MPa @Temperature 1095 °C |
1000 psi @Temperature 2003 °F |
Cold Crush Strength |
BNZ Materials Blazecrete 2600 Dense Castable Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as.. |